I-Metal Foam inezici ze-porosity ephezulu, indawo enkulu ethize, i-ductility enhle kanye ne-thermal conductivity ephezulu, futhi inezindawo ezinhle ze-hydrodynamic. Inezinzuzo ezibaluleke kakhulu ekuphenduleni kwe-catalytic kwamagesi noketshezi. Ekuphenduleni kwe-catalytic, insimbi esekelwe ku-nickel enegwebu noma i-copper-based ingasetshenziswa ngokuqondile njenge-catalyst, noma insimbi enegwebu ingasetshenziswa njengesithwali se-catalyst, futhi ezinye izisusa zingaxhunywa kungqimba olungaphezulu. Isetshenziswa ku-catalysis yezindlela ezintathu zokuphuma kwemoto, ukusabela kwamakhemikhali ezokwelapha, njll.
Imininingwane Yomkhiqizo:
| Uhlobo | Vula iseli |
| Ubumsulwa | > 99% |
| Ifomu | Ishidi noma Roll, kuye ngosayizi & ukujiya |
| Usayizi Weseli (PPI) | 10-150PPI, ngokwesicelo ngasinye |
| Ubukhulu | Okujwayelekile: 1-30mm Mncane Kakhulu (30mm) lungenziwa ngokwezifiso njengesicelo |
| Usayizi Nomumo | Okujwayelekile: 500 * 500mm/ 200 * 300mm; ingenziwa ngendlela ehlukile ngokwesicelo ngasinye |
| I-Porosity | 95%-98% |
| Vula Isilinganiso Seseli | ≥98 % |
| Ukuminyana Kwevolumu | >0.1g/cm3, ngokwesicelo ngasinye |
| Ukuminyana kobuso | 200-2500 g/m ^2, ngokwesicelo ngasinye |
| I-Thermal Conductivity (Theory) | >3W/MK |
| Amandla Emishini (Theory) | ≥2~7MPa |
| Amandla Okuqina (ngokwethiyori) | 8 ~ 50MPa |
| Ukumelana Nezinga lokushisa (Okungokwethiyori) | ≥500℃ |
| Isisindo samangqamuzana | 58.68 |
| I-Melting Point | 1455 °C |
| Iphuzu elibilayo | 2732 °C |
| Ukushisa Okuthize | 0.44 kJ/kg·K |
| Vickers Ukuqina | 638 MPa |
| Ukuminyana kwe-areal | 350±20g/m2 |
| I-conductivity kagesi | 69.3 nΩ·m (20 °C) |
Isikhathi sokuthumela: Sep-23-2022